Er3+ 掺杂对Bi3Ti1.5W0.5O9-Bi4Ti3O12 共生无铅压电陶瓷性能的影响
曾仁芬, 江向平, 陈超, 黄枭坤, 聂鑫, 叶芬

Effects of Er3+-doping on Performance of Bi3Ti1.5W0.5O9-Bi4Ti3O12 Intergrowth Lead-free Piezoceramics
ZENG Renfen, JIANG Xiangping, CHEN Chao, HUANG Xiaokun, NIE Xin, YE Fen
图1 BTW-BIT-xEr3+陶瓷在室温下的XRD图谱和BTW-BIT-xEr3+陶瓷在衍射角2θ在29°~30.5°范围的放大图
Fig.1 XRD patterns for BTW-BIT-xEr3+ ceramics at room temperature (a) and enlargement of BTW-BIT-xEr3+ ceramics with diffraction angle 2θ in the range of 29°~30.5° (b)