用常压空气等离子体对PBO纤维表面接枝改性
陈怿咨, 张承双, 陈平

Surface Graft Modification of Domestic PBO Fiber by Atmospheric Air Plasma
CHEN Yizi, ZHANG Chengshuang, CHEN Ping
表6 带有上浆剂的PBO纤维接枝前后的峰强比
Table 6 Strength ratio of PBO fiber (with sizing agent) groups before and after being grafted (%)
SampleI844/I818d(PBO)I924/I818d(PBO)I924/I844d(PBO)
PBO94.17-61.16-64.95-
DBD94.340.1775.4814.3280.0115.06
HDIE95.030.8660.30-0.8763.45-1.50
HDITE94.190.0261.730.5665.540.59
HMDIE96.151.9862.130.9664.61-0.34
HDMITE94.840.6760.06-1.1063.33-1.62
IPDIE94.550.3861.790.6365.350.40
IPDITE95.070.9079.2318.0783.3418.39