汽轮机转子10%Cr钢的高温低周疲劳特性 |
崔璐, 康文泉, 邹方, 魏文澜, 李臻, 王澎 |
High Temperature Low Cycle Fatigue Characteristics of Steam Turbine Rotor Steel 10%Cr |
CUI Lu, KANG Wenquan, ZOU Fang, WEI Wenlan, LI Zhen, WANG Peng |
图9 高温低周疲劳的最大裂纹长度随循环周期的变化趋势 |
Fig.9 Maximum crack length evolution under high tem-perature LCF conditions (T=600℃, Δε=1.1%) for 10%Cr |
![]() |