长期时效对低膨胀高温合金GH2909性能的影响 |
徐雄, 李钊, 万志鹏, 韦康, 王涛, 张新房 |
Effect of Long-term Aging on Properties of Low Expansion Superalloy GH2909 |
XU Xiong, LI Zhao, WAN Zhipeng, WEI Kang, WANG Tao, ZHANG Xinfang |
图10 合金在650℃长期时效2000 h后室温拉伸断口的纵剖SEM形貌 |
Fig.10 SEM morphology longitudinal section at room temperature after long-term aging at 650℃ for 2000 h |
![]() |