镍基高温合金定向凝固用陶瓷型壳粘砂反应
|
石振威, 郑伟, 卢玉章, 张功, 申健
|
Sand-burning Reaction of Ceramic Shell for Directional Solidification of Nickel-based Superalloy
|
SHI Zhenwei, ZHENG Wei, LU Yuzhang, ZHANG Gong, SHEN Jian
|
|
表6 各指标的极差结果
|
Table 6 Range analysis of various indicators
|
|
Indicator | Factor | K1 | K2 | K3 | R |
---|
Sand-burning proportion/% | A | 6.46 | 13.60 | 14.12 | 7.66 | B | 11.29 | 10.35 | 12.54 | 2.19 | C | 6.59 | 15.32 | 12.27 | 8.73 | D | 12.18 | 9.58 | 12.42 | 2.84 | Surface roughness Ra/μm | A | 6.91 | 7.75 | 8.00 | 1.09 | B | 8.27 | 6.04 | 8.35 | 2.31 | C | 7.04 | 7.66 | 7.95 | 0.91 | D | 7.07 | 8.23 | 7.36 | 1.16 | Porosity/% | A | 20.29 | 48.07 | 67.27 | 46.98 | B | 43.20 | 47.74 | 44.69 | 4.54 | C | 46.16 | 51.87 | 37.60 | 14.27 | D | 50.46 | 39.49 | 45.68 | 10.97 |
|
|
|