盐雾预腐蚀对HRB400E抗震钢筋超低周疲劳性能的影响
谌理飞, 罗云蓉, 张应迁, 李辉, 李秀兰, 廖文丽

Effect of Pre-corrosion by Salt Spray on Extremely Low Cycle Fatigue Performance of HRB400E Seismic Steel Bar
CHEN Lifei, LUO Yunrong, ZHANG Yingqian, LI Hui, LI Xiulan, LIAO Wenli
表4 ELCF参数
Table 4 ELCF parameters
Corrosion time/dεf'c

σf'

/MPa

b

k'

/MPa

n'
00.2-0.56200-0.1410240.18
300.22-0.54400-0.0849900.18
600.132-0.44000-0.0811980.22
900.12-0.373184-0.03711890.24