盐雾预腐蚀对HRB400E抗震钢筋超低周疲劳性能的影响
谌理飞, 罗云蓉, 张应迁, 李辉, 李秀兰, 廖文丽

Effect of Pre-corrosion by Salt Spray on Extremely Low Cycle Fatigue Performance of HRB400E Seismic Steel Bar
CHEN Lifei, LUO Yunrong, ZHANG Yingqian, LI Hui, LI Xiulan, LIAO Wenli
表1 HRB400E钢筋的化学成分(质量分数,%)
Table 1 Chemical composition of HRB400E steel bar (mass fraction, %)
SSiMnCPFe
0.0290.3401.4400.2200.021Bal.