表面划伤对690TT合金传热管腐蚀行为的影响 |
孟凡江, 吴斌, 吕云鹤, 明洪亮, 鲍一晨, 王俭秋, 韩恩厚 |
Effect of Surface Scratch on Corrosion Behavior of Alloy 690TT Heat Exchanger Tubes |
MENG Fanjiang, WU Bin, LV Yunhe, MING Hongliang, BAO Yichen, WANG Jianqiu, HAN En-Hou |
图8 划伤深度为30 μm、70 μm、110 μm试样腐蚀2000 h后截面的形貌 |
Fig.8 Cross-sectional morphologies of scratched samples with the scratch depth of 30 μm,70 μm and 110 μm after 2000 h corrosion (a1~a3) scratched groove; (b1~b3) left scratch bank; (c1~c3) right scratch bank |
![]() |