定向凝固Ti-(43-48)Al-2Cr-2Nb合金的显微组织和性能
|
Microstructure and Properties of Ti-(43-48)Al-2Cr-2Nb Alloy Prepared by Directional Solidification
|
图5. 抽拉速度为0.6 mm/min的Ti-(43-48)Al-2Cr-2Nb合金定向凝固纵剖面的显微组织 |
Fig.5. Lognitudinal macrostructures of directionally solidified Ti-45Al-2Cr-2Nb alloys under drawing rate of 0.6 mm/min (a) Ti-43Al-2Cr-2Nb; (b) Ti-45Al-2Cr-2Nb; (c) Ti-48Al-2Cr-2Nb |
![]() |