Inconel 600合金中不同类型晶界处铬的浓度
郑合凤, 师梦杰, 毛强, 张孟超, 李慧()
Chromium Concentration Near Grain Boundaries with Various Characters in Inconel Alloy 600
ZHENG Hefeng, SHI Mengjie, MAO Qiang, ZHANG Mengchao, LI Hui()

图1. 600合金样品在1100℃固溶处理15 min、固溶处理后冷轧5%、再在1100℃再结晶退火5 min(GBE)后的OIM图,以及固溶处理和GBE处理的样品中不同类型晶界特征分布统计图(Palumbo-Aust标准[13],长度百分比)

Fig.1. OIM maps of Alloy 600 samples (a) solution treated at 1100℃ for 15 min, (b) and then is cold-rolled 5%, recrystallized at 1100℃ for 5 min, and (c) grain boundary character distribution statistics (Palumbo-Aust criterion[13], length fraction) of solution treatment and GBE treated samples