Q345q桥梁钢和Q345qNH耐候钢在模拟工业大气+除冰盐混合介质中的腐蚀行为
郭铁明1,2(), 徐秀杰1,2, 张延文1,2, 宋志涛1,2, 董志林1,2, 金玉花1,2
Corrosion Behavior of Q345q Bridge Steel and Q345qNH Weathering Steel in a Mixed Medium of Simulated Industrial Environment Solution and Deicing Salt
GUO Tieming1,2(), XU Xiujie1,2, ZHANG Yanwen1,2, SONG Zhitao1,2, DONG Zhilin1,2, JIN Yuhua1,2

图6. 两种钢腐蚀480 h后截面的SEM照片

Fig.6. SEM images of cross-sections of two steels after corrosion for 480 h (a) Q345qNH, (b) Q345q