Bi对Mg-3Al-3Nd合金显微组织和力学性能的影响
|
|
Effect of Bi on Microstructure and Mechanical Properties of Mg-3Al-3Nd Alloy
|
|
图 10. Mg-3Al-3Nd-xBi合金的高温拉伸断口形貌 |
Fig.10. High temperature tensile fracture morphology of Mg-3Al-3Nd-xBi alloy (a) Mg-3Al-3Nd; (b) Mg-3Al-3Nd-1Bi; (c) Mg-3Al-3Nd-2Bi; (d) Mg-3Al-3Nd-3Bi |
![]() |