SiC泡沫陶瓷/球墨铸铁双连续相复合材料的气固两相流冲蚀性能
万伟1,2, 曹小明1, 张劲松1()
Erosion Performance for Co-continuous Phase Composite of SiC Foam Ceramic/Ductile Iron
WAN Wei1,2, CAO Xiaoming1, ZHANG Jinsong1()

图9. SiCfoam/DI复合材料α=30°、ν=100 m/s时的冲蚀形貌

Fig.9. Erosion morphology of SiCfoam/DI composites at α=30° and ν=100 m/s