SiC泡沫陶瓷/球墨铸铁双连续相复合材料的气固两相流冲蚀性能
万伟1,2, 曹小明1, 张劲松1()
Erosion Performance for Co-continuous Phase Composite of SiC Foam Ceramic/Ductile Iron
WAN Wei1,2, CAO Xiaoming1, ZHANG Jinsong1()

图7. α=30°、ν=75 m/s和α=90°、ν=75 m/s时DI的冲蚀形貌

Fig.7. Erosion appearance of DI erosion at α=30° and ν=75 m/s (a) (b), at α=90° and ν=75 m/s (c)