热处理时间对透辉石系尾矿微晶玻璃析晶及其性能的影响
|
Influences of Heat Treatment Soaking Time on Crystallization and Properties of Tailings-based Glass-Ceramics
|
图4. 用传统法在820℃保温不同时间制备的微晶玻璃的SEM照片 |
Fig.4. SEM images of as-synthesized glass-ceramics at 820℃ with different soaking time by conventional heating (a) C0G-820℃/0 min, (b) C15G-820℃/15 min, (c) C30G-820℃/30 min, (d) C45G-820℃/45 min |
![]() |