热处理时间对透辉石系尾矿微晶玻璃析晶及其性能的影响
|
Influences of Heat Treatment Soaking Time on Crystallization and Properties of Tailings-based Glass-Ceramics
|
图3. 用传统法在720℃保温不同时间制备的微晶玻璃的SEM照片 |
Fig.3. SEM images of as-synthesized glass-ceramics at 720℃ with different soaking time by conventional heating (a) C20D-720℃/20 min, (b) C30D-720℃/30 min, (c) C60HD-720℃/1 h, (d) C120HD-720℃/2 h |
![]() |