热处理时间对透辉石系尾矿微晶玻璃析晶及其性能的影响
|
Influences of Heat Treatment Soaking Time on Crystallization and Properties of Tailings-based Glass-Ceramics
|
图5. 在720℃保温不同时间制备的微晶玻璃的XRD图谱 |
Fig.5. XRD patterns of glass-ceramics heat treated at 720℃ for different soaking times |
![]() |