		含缺陷的Al-Si-Mg合金的疲劳性能和强度评估
		 | 
| 
			Fatigue Properties and Strength Assessment for Al-Si-Mg Alloy via Test Samples with Artificial Defects
			 | 
| 图4. 不同尺寸钻孔试样的疲劳断口 | 
| Fig.4. Drilled specimen fatigue fracture in different sizes (a) 925 μm drilled specimen–70 MPa stress level; (b) 370 μm drilled specimen–90 MPa stress level | 
|  |