MgCl2对锌在干湿交替环境中腐蚀行为的影响 |
||||||||||||
尹奇,刘淼然,刘雨薇,潘晨,王振尧 | ||||||||||||
Effect of MgCl2 Deposite on Simulated Atmospheric Corrosion of Zn via Wet-dry Altertnating Corrosion Test |
||||||||||||
Qi YIN,Miaoran LIU,Yuwei LIU,Chen PAN,Zhenyao WANG | ||||||||||||
表4 不同组中腐蚀产物Zn5(OH)8Cl2·H2O的主峰位置与基体Zn主峰位置 | ||||||||||||
Table 4 Main peak position of Zn5(OH)8Cl2·H2O and Zn in the experimental groups | ||||||||||||
|
||||||||||||