用原位聚合法制备的PA6/GO纳米复合材料的结构和性能
黄欢,陈宇哲,郭怡,蔺海兰,王丽君,马素德,卞军,谷志杰

Structure and Properties of PA6/GO Nanocomposite by In-situ Polymerization
Huan HUANG,Yuzhe CHEN,Yi GUO,Hailan LIN,Lijun WANG,Sude MA,Jun BIAN,Zhijie GU
表1 PA6/GO纳米复合材料的黏均分子量
Table 1 Viscosity average molecular weight of PA6/GO nanocomposites
SamplesViscosity average molecular weigh
PA63.23×104
C-A-G(100/10/0)2.98×104
C-A-G(100/10/0.05)2.94×104
C-A-G(100/10/0.1)3.02×104
C-A-G(100/10/0.2)2.91×104
C-A-G(100/10/0.4)2.94×104
C-A-G(100/10/0.8)2.85×104
C-A-G(100/10/1.0)2.64×104