在盐湖地区暴露48个月纯锌的腐蚀行为
张丹,王振尧()
Corrosion Behavior of Zinc Exposed to Salt Lake Area for 48 Months
Dan ZHANG,Zhenyao WANG()

图5. 暴晒不同时间后纯锌的截面形貌图

Fig.5. Skyward cross section morphologies of corrosion product layer of zinc after exposure for 6 (a), 12 (b), 24 (c) and 48 months (d), and the field-ward cross section morphologies of corrosion product layer of zinc for 6 (a'), 12 (b'), 24 (c') and 48 months (d')