在盐湖地区暴露48个月纯锌的腐蚀行为
张丹,王振尧()
Corrosion Behavior of Zinc Exposed to Salt Lake Area for 48 Months
Dan ZHANG,Zhenyao WANG()

图3. 暴晒不同时间后纯Zn的表面形貌

Fig.3. Skyward surface appearances of zinc after exposure for 6 (a), 12 (b), 24 (c) and 48 months (d), and the field-ward surface appearances for 6 (a'), 12 (b'), 24 (c') and 48 months (d')