预嵌锂多壁碳纳米管的性能
陈玮,聂艳艳,孙晓刚,李旭,王杰,胡浩,梁国东,黄雅盼,魏成成

Performance of Lithium-ion Capacitors Using Pre-lithiated Multi-walled Carbon Nanotube Composite Anode
Wei CHEN,Yanyan NIE,Xiaogang SUN,Xu LI,Jie WANG,Hao HU,Guodong LIANG,Yapan HUANG,Chengcheng WEI
表1 锂离子电容器在不同电流密度下的功率密度和能量密度以及比电容数据
Table 1 Specific capacitance, power density and energy density data of LICs with different current density

Current density

mA·g-1

PrimitivePre-lithiated

CSP

F·g-1

ESP

Wh·kg-1

PSP

W·kg-1

CSP

F·g-1

ESP

Wh·kg-1

PSP

W·kg-1

5010.7417.5374.6185.18140.4074.70
1008.6613.86148.5175.91123.81149.02
2007.2811.30294.7773.32117.00296.42
5005.707.99719.1469.90104.29729.04
10005.236.141382.361.2681.171417.9
2000---54.6967.442790.6
3000---41.3343.924054.5
4000---34.9132.095250.7