纤维预热温度对连续Al2O3f/Al复合材料力学性能的影响
胡银生,余欢,徐志锋(),蔡长春,聂明明
Effect of Fiber Preheating Temperature on Mechanical Properties of Continuous Al2O3f/Al Composites
Yinsheng HU,Huan YU,Zhifeng XU(),Changchun CAI,Mingming NIE

图12. 不同预热温度的连续Al2O3f/ZL210A拉伸断口的形貌

Fig.12. Continuous Al2O3f/ZL210A tensile fracture surface with different preheating temperatures (a, b) 500℃; (c, d) 530℃; (e, f) 560℃; (g, h) 600℃