纤维预热温度对连续Al2O3f/Al复合材料力学性能的影响
|
Effect of Fiber Preheating Temperature on Mechanical Properties of Continuous Al2O3f/Al Composites
|
图6. 不同状态下Al2O3纤维的表面形貌 |
Fig.6. Surface morphology of Al2O3 fibers in different states (a) Raw silk; (b) treated by 500℃ and NaOH;(c) Extracted from Al2O3f/Al composite at 500℃ preheating temperatures; (d) Extracted from Al2O3f/ Al composite at 530℃ preheating temperatures; (e) Extracted from Al2O3f/ Al composite at 560℃ preheating temperatures; (f) Extracted from Al2O3f/ Al composite at 600℃ preheating temperatures |
![]() |