烧结温度对TC4合金的微观结构和力学性能的影响
杨军,张家敏,马文瑾,杜立辉,易健宏,甘国友,游昕,李凤仙

Effect of Sintering Temperature on Microstructure and Mechanical Properties of TC4 Alloy
Jun YANG,Jiamin ZHANG,Wenjin MA,Lihui DU,Jianhong YI,Guoyou GAN,Xin YOU,Fengxian LI
表1 试样烧结前后的相对密度
Table 1 Relative density of samples before and after sintering (%)

Sintering

temperature

1.5 h2.0 h2.5 h
Before sintering After sinteringBefore sintering After sinteringBefore sintering After sintering
1100℃62.7396.9158.6598.6162.2399.06
1150℃58.9697.4258.7898.7762.2999.19
1200℃65.0399.0260.1799.0260.4899.58