TB6钛合金β区变形的动态再结晶动力学
欧阳德来1,鲁世强1,崔霞1(),徐勇1,杜海明2,朱慧安1
Kinetics of Dynamic Recrystallization of TB6 Ti-Alloy During Hot Compressive Deformation atTemperatures of β-phase Range
Delai OUYANG1,Shiqiang LU1,Xia CUI1(),Yong XU1,Haiming DU2,Huian ZHU1

图6. TB6钛合金在变形温度为825℃、应变速率为0.001 s-1条件下的应力-应变曲线和θ-σ曲线

Fig.6. Stress-strain curves (1-True curve, 2-Fitting curve) (a) and θ~σ curve (1-True curve, 2-Extrapolation curve) (b) of TB6 titanium alloy at deformation temperature 825℃ and strain rate 0.001 s-1