8.8级螺栓用ML40Cr钢的疲劳性能和裂纹扩展行为
王源晨1,宋竹满1,李瑞2,史文博3,朱艳坤1,张广平1()
Fatigue Properties and Crack Growth Behavior of ML40Cr Steel for 8.8-grade Bolts
WANG Yuanchen1,SONG Zhuman1,LI Rui2,SHI Wenbo3,ZHU Yankun1,ZHANG Guangping1()

图1. 光滑疲劳试样、缺口疲劳试样和单边缺口疲劳试样的尺寸示意图

Fig.1. Dimensions of smooth fatigue specimen (a), notched fatigue specimen (b) and single-edge notched specimen (c) (unit: mm)