带氧化皮Q345q钢在模拟西北典型大气环境中的腐蚀行为研究
张延文1,2,郭铁明1,2(),宋志涛1,2,南雪丽1,2,徐秀杰1,2,董志林1,2
Corrosion Behavior of Q345q Steel with Oxide Scale in Simulated Typical Atmospheric Environmentin Northwest China
ZHANG Yanwen1,2,GUO Tieming1,2(),SONG Zhitao1,2,NAN Xueli1,2,XU Xiujie1,2,DONG Zhilin1,2

图8. 带氧化皮Q345q钢在3种溶液中腐蚀不同时间的截面形貌

Fig.8. Cross-sectional morphologies of Q345q steel with oxide scale after corrosion in (a~c) deicing salt, (d~f) NaHSO3 and (g~i) deicing salt+NaHSO3 solutions for (a, d, g) 24 h, (b, e, h) 192 h and (c, f, i) 288 h