核用SA508-4N钢粗晶区再热裂纹敏感性评价
|
Reheat Cracking Susceptibility in Coarse Grained Heat-affected Zone of SA508-4 Steel for Nuclear Pressure Vessel
|
图7. 不同参数条件下钢裂纹扩展处的空洞 |
Fig.7. Voids in the direction of crack propagation of steel for different parameters (a) Steel A-550℃-50 s, (b) Steel B-550℃-50 s, (c) Steel A-610℃-50 s, (d) Steel B-610℃-50 s |
![]() |