双连续Si3N4/1Cr18Ni9Ti复合材料的制备和冲蚀性能
杜奇1,2,高勇1,任志恒1,3,曹小明1,王超1,张劲松1()
Preparation and Erosion Performance for Co-continuous Phase Composites of Si3N4/1Cr18Ni9Ti
Qi DU1,2,Yong GAO1,Zhiheng REN1,3,Xiaoming CAO1,Chao WANG1,Jinsong ZHANG1()

图11. 双连续Si3N4/1Cr18Ni9Ti复合材料的冲蚀机理示意图

Fig.11. Erosion mechanism of Si3N4/1Cr18Ni9Ti co-continuous composites (a) 8 h, (b) 16 h, (c) 24 h, (d) 32 h