双连续Si3N4/1Cr18Ni9Ti复合材料的制备和冲蚀性能
杜奇1,2,高勇1,任志恒1,3,曹小明1,王超1,张劲松1()
Preparation and Erosion Performance for Co-continuous Phase Composites of Si3N4/1Cr18Ni9Ti
Qi DU1,2,Yong GAO1,Zhiheng REN1,3,Xiaoming CAO1,Chao WANG1,Jinsong ZHANG1()

图10. 复合材料冲蚀前后高度差

Fig.10. Height difference of composite before and after erosion (a) Si3N4 area, (b) 1Cr18Ni9Ti area