TC11钛合金中 α''相和α'相的组织演变和显微硬度
张英东,李阁平,刘承泽,袁福森,韩福洲,Ali Muhanmmad,顾恒飞

Microstructure Evolution of α''-Phase and α'-Phase and Microhardness of TC11 Titanium Alloy
Yingdong ZHANG,Geping LI,Chengze LIU,Fusen YUAN,Fuzhou HAN,Muhanmmad Ali,Hengfei GU
图5 在不同温度固溶处理的TC11钛合金的XRD谱图
Fig.5 XRD patterns of TC11 titanium alloy solution treated at different temperature (a) 935℃, (b) 955℃, (c) 965℃, (d) 975℃, (e) 980℃, (f) 985℃, (g) 990℃, (h) 995℃