单晶高温合金凝固特性与典型凝固缺陷研究
|
ADVANCES IN SOLIDIFICATION CHARACTERISTICS AND TYPICAL CASTING DEFECTS IN NICKEL-BASED SINGLE CRYSTAL SUPERALLOYS
|
图13. C, B和Re含量不同的合金在叶片模拟件平台处杂晶的形成[37] |
Fig.13. Photograph of blade model at platform after macrocorrosion for alloy 1-1 (a), alloy 1-2 (b), alloy 2-1 (c), alloy 2-2 (d), alloy 3-1 (e), alloy 3-2 (f) and sampling position (g) (V=100 mm/s)[37] |
![]() |