O, N和Ni含量对0Cr25Ni7Mo4N双相不锈钢热轧塑性的影响*
|
陈雨来, 张泰然, 王一德, 李静媛
|
EFFECTS OF O, N AND Ni CONTENTS ON HOT PLASTICITY OF 0Cr25Ni7Mo4N DUPLEX STAINLESS STEEL
|
CHEN Yulai, ZHANG Tairan, WANG Yide, LI Jingyuan
|
|
表1 实验钢及SAF 2507双相不锈钢的化学成分 |
Table 1 Chemical compositions of tested steels and SAF 2507 steel |
|
Steel | C | Cr | Ni | Mo | Mn | Si | N | P | S | Al | O | Fe | No.1 | 0.027 | 25.3 | 6.72 | 4.18 | 0.65 | 0.66 | 0.25 | 0.025 | 0.0040 | 0.098 | 0.0059 | Bal. | No.2 | 0.015 | 24.7 | 8.33 | 4.06 | 0.08 | 0.16 | 0.34 | 0.012 | 0.0067 | 0.093 | 0.038 | Bal. | No.3 | 0.012 | 23.9 | 6.43 | 4.38 | 0.17 | 0.18 | 0.29 | 0.011 | 0.0076 | 0.120 | 0.0465 | Bal. | SAF 2507 | ≤0.03 | 24.0~ | 6.0~ | 3.0~ | ≤1.2 | ≤1.0 | 0.24~ | ≤0.035 | - | - | - | Bal. | | | 26.0 | 8.0 | 5.0 | | | 0.32 | | | | | |
|
|
|