42CrMo钢车轮锻件在淬火过程中的残余应力研究*
|
李永奎, 陈俊丹, 陆善平
|
RESIDUAL STRESS IN THE WHEEL OF 42CrMo STEEL DURING QUENCHING
|
LI Yongkui, CHEN Jundan, LU Shanping
|
|
|
表2 42CrMo钢的热物性参数 |
|
Temperature ℃ | Elastic modulus 105 MPa | Poisson's ratio | Specific heat Jkg-1℃-1 | Thermal expansion 10-6 ℃-1 | Thermal conductivity Wm-1℃-1 | 20 | 2.08 | 0.29 | - | - | - | 100 | 2.05 | 0.29 | 546 | 11.9 | 35.1 | 200 | 1.98 | 0.29 | 563 | 12.5 | 35.1 | 300 | 1.91 | 0.30 | 580 | 12.9 | 35.1 | 400 | 1.85 | 0.30 | 631 | 12.9 | 35.2 | 500 | 1.78 | 0.30 | 720 | 13.3 | 34.9 | 600 | 1.68 | 0.31 | 730 | 13.6 | 32.0 | 700 | 1.53 | 0.31 | 795 | 13.9 | 27.9 | 800 | 1.32 | 0.32 | 539 | 10.6 | 21.1 | 900 | 1.11 | 0.34 | 588 | 12.0 | 24.2 | 1000 | 1.04 | 0.34 | 591 | 13.0 | 24.5 |
|
|
|