材料研究学报. 2017, 31 (6): 409-414 doi: 10.11901/1005.3093.2016.267



时效处理对Ti-3Al-8V-6Cr-4Mo-4Zr合金力学性能的影响
王雪萌,张思倩,袁子尧,陈立佳

Effect of Heat Treatment on Mechanical Properties of Ti-3Al-8V-6Cr-4Mo-4Zr Alloy
Xuemeng WANG,Siqian ZHANG,Ziyao YUAN,Lijia CHEN
图4 Ti-3Al-8V-6Cr-4Mo-4Zr合金在不同状态下拉伸变形后的显微组织
Fig.4 TEM images of microstructure in different heat treatment conditions (a), (b) 800℃/30 min+500℃/8 h; (c), (d) 800℃/30 min+500℃/12 h;(e), (f) 800℃/30 min+500℃/24 h